EN 388 2016 Results: 3131XX Abrasion: 3 Cut (Coupe Test): 1 Tear: 3 Puncture: 1 Cut (TDM-100 Test): X Impact Protection: X
EN 388 is a European Standard. Cut Level is determined by the number of cycles it takes a spinning circular blade, that is pulled across the material under a constant weight of 500 grams, to cut the fabric. As the number of cycles increase, so does the glove's ratings. Click here for more information about the EN 388 2016 standard.
EN 388 2016 Results: 4121XX Abrasion: 4 Cut (Coupe Test): 1 Tear: 2 Puncture: 1 Cut (TDM-100 Test): X Impact Protection: X
EN 388 is a European Standard. Cut Level is determined by the number of cycles it takes a spinning circular blade, that is pulled across the material under a constant weight of 500 grams, to cut the fabric. As the number of cycles increase, so does the glove's ratings. Click here for more information about the EN 388 2016 standard.
EN 388 2016 Results: 4121XX Abrasion: 4 Cut (Coupe Test): 1 Tear: 2 Puncture: 1 Cut (TDM-100 Test): X Impact Protection: X
EN 388 is a European Standard. Cut Level is determined by the number of cycles it takes a spinning circular blade, that is pulled across the material under a constant weight of 500 grams, to cut the fabric. As the number of cycles increase, so does the glove's ratings. Click here for more information about the EN 388 2016 standard.
EN 388 2016 Results: 2131XX Abrasion: 2 Cut (Coupe Test): 1 Tear: 3 Puncture: 1 Cut (TDM-100 Test): X Impact Protection: X
EN 388 is a European Standard. Cut Level is determined by the number of cycles it takes a spinning circular blade, that is pulled across the material under a constant weight of 500 grams, to cut the fabric. As the number of cycles increase, so does the glove's ratings. Click here for more information about the EN 388 2016 standard.